dc.description276-279en_US
dc.description.abstractThe iron content was removed from crude wet process phosphoric acid produced by treating the Abu-Tartor phosphate ore with sulphuric acid, using potassium ferrocyanide as a precipitating agent. The iron content in the phosphoric acid filtrate is determined as ferric oxide by titration with K2Cr2O7 and using barium diphenyl amine sulphonate solution as indicator. The precipitates were washed, dried and converted to ferric oxide by heating at 100°C for 3 h. A sample of both the ferric -ferrocyanide and ferric oxide were characterized by using X-ray diffraction. It was found that the weight of the ferric ferrocyanide precipitate increases as the volume of the potassium ferrocyanide increases while the iron content in the phosphoric filtrate decreases. The results indicate that 30 kgm of potassium ferrocyanide is enough to precipitate about 60% of the original iron content in 1.46 ton of phosphoric acid with 8.2% loss in P2O5 from the original percentage.en_US
dc.language.isoen_USen_US
dc.publisherNISCAIR-CSIR, Indiaen_US
dc.rights CC Attribution-Noncommercial-No Derivative Works 2.5 Indiaen_US
dc.sourceIJCT Vol.06(5) [September 1999]en_US
dc.titleReducing iron content in crude phosphoric acid by potassium ferrocyanideen_US
dc.typeArticleen_US
Appears in Collections:IJCT Vol.06(5) [September 1999]

Files in This Item:
File Description SizeFormat 
IJCT 6(5) 276-279.pdf820.21 kBAdobe PDFView/Open


Items in NOPR are protected by copyright, with all rights reserved, unless otherwise indicated.