Please use this identifier to cite or link to this item: http://nopr.niscpr.res.in/handle/123456789/17105
Full metadata record
DC FieldValueLanguage
dc.contributor.authorNadolny, Krzysztof-
dc.contributor.authorKapłonek, Wojciech-
dc.contributor.authorWojtewicz, Michal-
dc.date.accessioned2013-04-18T07:36:53Z-
dc.date.available2013-04-18T07:36:53Z-
dc.date.issued2013-04-
dc.identifier.issn0975-1017 (Online); 0971-4588 (Print)-
dc.identifier.urihttp://hdl.handle.net/123456789/17105-
dc.description108-124en_US
dc.description.abstractThis paper presents an assessment of the influence exerted upon the internal cylindrical grinding of Titanium Grade 2® by the sulfurization of grinding wheels with ceramic bond. The sulfurization method of ceramic grinding wheels is presented against the background of a chemical basis for abrasive machining. The experimental investigation methodology is described. It includes a presentation of the proposed method for comparison of the sulfurization influence on the grinding results, which consists in performing a short grinding test in the plunge grinding kinematics. The paper emphasizes the multicriterial analysis of the experimental test results. It also describes the condition of the grinding wheel active surface (GWAS) that has not been sulfurized and one that has been impregnated with sulfur after grinding of the Titanium Grade 2®. The assessment has been carried out on the basis of the acquired SEM micrographs, as well as measurements of the surface microtopography with an optical profilometer and laser scatterometry method. The paper also analyzes the workpiece surface roughness measured with the stylus profilometry method, as well as the elemental composition of the surface inclusions, using Energy Dispersive X-ray Spectroscopy (EDS). The experimental results show that impregnation with sulfur makes it possible to significantly limit the phenomenon of smearing the GWAS with the machined material. en_US
dc.language.isoen_USen_US
dc.publisherNISCAIR-CSIR, Indiaen_US
dc.rights CC Attribution-Noncommercial-No Derivative Works 2.5 Indiaen_US
dc.sourceIJEMS Vol.20(2) [April 2013]en_US
dc.subjectGrinding processen_US
dc.subjectSulfurizationen_US
dc.subjectGrinding wheelsen_US
dc.subjectInternal cylindrical grindingen_US
dc.subjectSurface roughnessen_US
dc.titleEffects of sulfurization of grinding wheels on internal cylindrical grinding of Titanium Grade 2®en_US
dc.typeArticleen_US
Appears in Collections:IJEMS Vol.20(2) [April 2013]

Files in This Item:
File Description SizeFormat 
IJEMS 20(2) 108-124.pdf1.58 MBAdobe PDFView/Open


Items in NOPR are protected by copyright, with all rights reserved, unless otherwise indicated.