Please use this identifier to cite or link to this item: http://nopr.niscpr.res.in/handle/123456789/22672
Title: Alkali deweighting of acid-modified multicomponent copolyester fibre
Authors: Yang, Ruxin
Keywords: Multicomponent copolyester fibre;Alkali peeling;Alkali deweighting;Copolyester fibre
Issue Date: Sep-2003
Publisher: NISCAIR-CSIR, India
Abstract: The treatment conditions for alkali deweighting of acid-modified multicomponent copolyester fibres have been optimized. The satisfactory silk- like effect is observed under the specific treatment conditions [7.5g/L NaOH, 85°C temperature, 40 min treatment time, 1:40 material-to-liquor ratio, and 1.0g/L promoter]. After alkali deweighting, the special micro-pit structure occurs on the surface of acid-modified fibres which enhances the fibre permeability, adhesion regain, capability of colouring and feel. The X-ray diffraction patterns show that the degree of crystallization of fibre decreases after alkali peeling.
Page(s): 343-347
ISSN: 0975-1025 (Online); 0971-0426 (Print)
Appears in Collections:IJFTR Vol.28(3) [September 2003]

Files in This Item:
File Description SizeFormat 
IJFTR 28(3) 343-347.pdf1.06 MBAdobe PDFView/Open


Items in NOPR are protected by copyright, with all rights reserved, unless otherwise indicated.