Please use this identifier to cite or link to this item:
http://nopr.niscpr.res.in/handle/123456789/22990Full metadata record
| DC Field | Value | Language |
|---|---|---|
| dc.contributor.author | Naik, Y Arthoba | - |
| dc.contributor.author | Venkatesha, T V | - |
| dc.contributor.author | Nayak, P Vasudeva | - |
| dc.date.accessioned | 2013-10-31T12:05:48Z | - |
| dc.date.available | 2013-10-31T12:05:48Z | - |
| dc.date.issued | 2001-09 | - |
| dc.identifier.issn | 0975-0991 (Online); 0971-457X (Print) | - |
| dc.identifier.uri | http://hdl.handle.net/123456789/22990 | - |
| dc.description | 390-395 | en_US |
| dc.description.abstract | Zinc electroplating is carried out in
presence of condensation product formed between ![]() -Alanine and Glutaraldehyde. The bath
constituents are optimized through Hull
cell experiments. Operating parameters such as pH, temperature, current density
are also optimized. Current efficiency and throwing power are measured. Polarization
study reveals high shift of potential towards negative direction in the presence
of addition agents. Corrosion resistance test indicated good protection of steel
by the coating. IR spectrum of the deposit shows the inclusion of the compound.
SEM photomicrographs show fine grained deposit in the presence of addition agent.
The consumption of brightener in the lab scale is 8 mL for 1000 amp-hour. | en_US |
| dc.language.iso | en_US | en_US |
| dc.publisher | NISCAIR-CSIR, India | en_US |
| dc.rights | CC Attribution-Noncommercial-No Derivative Works 2.5 India | en_US |
| dc.source | IJCT Vol.08(5) [September 2001] | en_US |
| dc.title | Effect of condensation product on bright zinc electrodeposition from sulphate bath | en_US |
| dc.type | Article | en_US |
| Appears in Collections: | IJCT Vol.08(5) [September 2001] | |
Files in This Item:
| File | Description | Size | Format | |
|---|---|---|---|---|
| IJCT 8(5) 390-395.pdf | 1.21 MB | Adobe PDF | View/Open |
Items in NOPR are protected by copyright, with all rights reserved, unless otherwise indicated.

-Alanine and Glutaraldehyde. The bath
constituents are optimized through Hull
cell experiments. Operating parameters such as pH, temperature, current density
are also optimized. Current efficiency and throwing power are measured. Polarization
study reveals high shift of potential towards negative direction in the presence
of addition agents. Corrosion resistance test indicated good protection of steel
by the coating. IR spectrum of the deposit shows the inclusion of the compound.
SEM photomicrographs show fine grained deposit in the presence of addition agent.
The consumption of brightener in the lab scale is 8 mL for 1000 amp-hour.