Please use this identifier to cite or link to this item: http://nopr.niscpr.res.in/handle/123456789/23187
Title: Study on rotor deposition: Part II - Influence on quality and running performance of fibre dyed cotton yarn
Authors: Ishtiaque, S M
Das, A
Keywords: Cotton yarn;Crock fastness;End breakage rate;Residual trash content;Rotor deposition;Yarn CSP;Yarn imperfections;Yarn irregularity
Issue Date: Dec-2002
Publisher: NISCAIR-CSIR, India
Abstract: The residual trash content in finisher draw frame sliver of natural yellow and green dyed cotton slivers is found to be very high as compared to that in grey or reactive dyed slivers, which is due to the deposition of large dye particles over the surface of' fibres during dyeing. The residual trash content of natural indigo dyed sliver is very low, but the end breakage rate of indigo and green dyed is extremely high which is due to coating of rotor surface with colours because of the poor crock fastness of these two fibres. The quality of yarn also deteriorates due to the coating of rotor surface with colours. Blending of grey cotton sliver with natural indigo sliver at finisher draw frame stage shows improvement in spinnability and yarn quality.
Page(s): 381-387
ISSN: 0975-1025 (Online); 0971-0426 (Print)
Appears in Collections:IJFTR Vol.27(4) [December 2002]

Files in This Item:
File Description SizeFormat 
IJFTR 27(4) 381-387.pdf1.4 MBAdobe PDFView/Open


Items in NOPR are protected by copyright, with all rights reserved, unless otherwise indicated.