dc.description.abstractWrap-spun jute yarns of 276 tex linear density have been spun at different wrap densities (250,300,350, 400 and 450 wpm) using polypropylene, polyester and nylon of different linear densities as wrapping elements. It is observed that in the case of 23.3 tex polypropylene multifilament and 17.2 tex polyester multifilament wrappers, the yarn could not be spun beyond 350 wpm due to the excessive breakage of wrapping elements. The breaking strength of the wrap-spun jute yarn increases with the increase in wrap density up to an optimum level and then decreases. The breaking extension of the wrapspun jute yarns increases but initial modulus decreases with the increase in wrap density. en_US
dc.language.isoen_USen_US
dc.publisherNISCAIR-CSIR, Indiaen_US
dc.rights CC Attribution-Noncommercial-No Derivative Works 2.5 Indiaen_US
dc.sourceIJFTR Vol.26(3) [September 2001]en_US
dc.subjectBreaking extensionen_US
dc.subjectInitial modulusen_US
dc.subjectJuteen_US
dc.subjectNylonen_US
dc.subjectPolyesteren_US
dc.subjectPolypropyleneen_US
dc.subjectTenacityen_US
dc.subjectWork of ruptureen_US
dc.subjectWrap densityen_US
dc.subjectWrap-spun yarnen_US
dc.titleStudies on tensile responses of wrap-spun jute yarnen_US
dc.typeArticleen_US
Appears in Collections:IJFTR Vol.26(3) [September 2001]

Files in This Item:
File Description SizeFormat 
IJFTR 26(3) 246-250.pdf1.05 MBAdobe PDFView/Open


Items in NOPR are protected by copyright, with all rights reserved, unless otherwise indicated.