Please use this identifier to cite or link to this item: http://nopr.niscpr.res.in/handle/123456789/29806
Full metadata record
DC FieldValueLanguage
dc.contributor.authorBalakrishna, P-
dc.contributor.authorChakraborthy, K P-
dc.contributor.authorSingh, Ajit-
dc.date.accessioned2014-11-07T08:59:29Z-
dc.date.available2014-11-07T08:59:29Z-
dc.date.issued1996-10-
dc.identifier.issn0975-1017 (Online); 0971-4588 (Print)-
dc.identifier.urihttp://hdl.handle.net/123456789/29806-
dc.description196-200en_US
dc.description.abstractEnd-capping defect is one of the causes of rejection in pressed and sintered ceramic compacts. The causes of its occurrence lie both in the quality of the powder and that of pressing. In this paper, end-capping and other defects have been described and their relationship to powder characteristics and pressing parameters has been brought out. It is found that soft powders that are free from agglomerates, and well finished suitably tapered hard material dies and moderate compaction pressures tend to minimize end-capping and other defects.en_US
dc.language.isoen_USen_US
dc.publisherNISCAIR-CSIR, Indiaen_US
dc.rights CC Attribution-Noncommercial-No Derivative Works 2.5 Indiaen_US
dc.sourceIJEMS Vol.03(5) [October 1996]en_US
dc.titleEnd-capping and other defects in pressed ceramic compactsen_US
dc.typeArticleen_US
Appears in Collections:IJEMS Vol.03(5) [October 1996]

Files in This Item:
File Description SizeFormat 
IJEMS 3(5) 196-200.pdf402.15 kBAdobe PDFView/Open


Items in NOPR are protected by copyright, with all rights reserved, unless otherwise indicated.