Please use this identifier to cite or link to this item:
http://nopr.niscpr.res.in/handle/123456789/30924| Title: | Preparation of fine sized boehmite |
| Authors: | Sidheswaran, P Bhat, A N |
| Issue Date: | Jul-1997 |
| Publisher: | NISCAIR-CSIR, India |
| Abstract: | Preparation of boehmite of fine particle size (< 6 μ) was attempted by three different routes. Flash calcinations of gibbsite at about 325°C for 2 h gave the desired material. However, the other two methods, dehydration of pseudoboehmite (at 110°C) and hydrothermal neutralization of aluminate with acid gave boehmite of larger particle size (11 and 17 μ, D50). |
| Page(s): | 206-209 |
| ISSN: | 0975-0991 (Online); 0971-457X (Print) |
| Appears in Collections: | IJCT Vol.04(4) [July 1997] |
Files in This Item:
| File | Description | Size | Format | |
|---|---|---|---|---|
| IJCT 4(4) 206-209.pdf | 245.45 kB | Adobe PDF | View/Open |
Items in NOPR are protected by copyright, with all rights reserved, unless otherwise indicated.