http://nopr.niscpr.res.in/handle/123456789/31610| Title: | Recovery and utilization of wash water solids generated during ilmenite leaching operation |
| Authors: | George, J Nair, V V Ninan, G Nair, K |
| Keywords: | Wash water;Dispersion;Reducing strength;Calcined solids |
| Issue Date: | Jun-2015 |
| Publisher: | NISCAIR-CSIR, India |
| Abstract: | The solid content in the spent wash water generated during leaching operations in chloride process for the production of TiO2 pigment is not recovered and considered waste. A method is proposed for the recovery of the solids and enrichment of titanium values in these solids. The composition of the recovered and enriched solids is determined by atomic absorption spectroscopy and other analytical techniques. The samples are characterized using X-ray diffraction (XRD) and scanning electron microscope. (SEM). The pigmentary qualities of the recovered material are studied in enamel paint formulations and compared against commercial rutile TiO2 pigment. Partial replacement of the TiO2 pigment with the recovered material has not made any significant impact on the various characteristics studied and approached the commercial rutile TiO2 pigment standards. Also partial replacement realizes a TiO2 saving in enamel paint formulations. |
| Page(s): | 362-366 |
| ISSN: | 0975-1084 (Online); 0022-4456 (Print) |
| Appears in Collections: | JSIR Vol.74(06) [June 2015] |
Files in This Item:
| File | Description | Size | Format | |
|---|---|---|---|---|
| JSIR 74(6) 362-366.pdf | 123.79 kB | Adobe PDF | View/Open |
Items in NOPR are protected by copyright, with all rights reserved, unless otherwise indicated.