Please use this identifier to cite or link to this item: http://nopr.niscpr.res.in/handle/123456789/32467
Full metadata record
DC FieldValueLanguage
dc.contributor.authorGulrajani, M L-
dc.contributor.authorGupta, Sanjay-
dc.contributor.authorKapur, Veena-
dc.contributor.authorJain, Madhulika-
dc.date.accessioned2015-10-05T05:46:33Z-
dc.date.available2015-10-05T05:46:33Z-
dc.date.issued1993-09-
dc.identifier.issn0975-1025 (Online); 0971-0426 (Print)-
dc.identifier.urihttp://hdl.handle.net/123456789/32467-
dc.description135-138en_US
dc.description.abstractA solar oven designed for giving temperatures in the range of 110-115͘ᵒC has been used for the fixation of pigment prints on silk using low temperature cure catalysts. The colour values and fastness properties of samples printed with different catalysts and thickeners and cured in solar and electric ovens have been measured and compared. The effect of partial substitution of kerosene with a synthetic thickener has also been investigated. Prints cured in solar oven are comparable in colour values and fastness properties to those cured in electric oven at a higher temperature. Kerosene emulsion thickening gives good results with both tartaric acid and catalyst LCP. Tartaric acid, however, is better of the two catalysts.en_US
dc.language.isoen_USen_US
dc.publisherNISCAIR-CSIR, Indiaen_US
dc.rights CC Attribution-Noncommercial-No Derivative Works 2.5 Indiaen_US
dc.sourceIJFTR Vol.18(3) [September 1993]en_US
dc.subjectCatalyst LCPen_US
dc.subjectKerosene substitutionen_US
dc.subjectPigment printingen_US
dc.subjectPrint fixationen_US
dc.subjectSilk fabricen_US
dc.subjectSolar ovenen_US
dc.titleFixation of pigment prints on silk using a solar ovenen_US
dc.typeArticleen_US
Appears in Collections:IJFTR Vol.18(3) [September 1993]

Files in This Item:
File Description SizeFormat 
IJFTR 18(3) 135-138.pdf906.38 kBAdobe PDFView/Open


Items in NOPR are protected by copyright, with all rights reserved, unless otherwise indicated.