Please use this identifier to cite or link to this item: http://nopr.niscpr.res.in/handle/123456789/32696
Title: Modification of Poly (ethylene terephthalate) Fibre by Polymer Blending with Poly(butylene terephthalate) Fibre: Part II-Sequential Melt-blending and Spinning
Authors: Viswanath, C S
Deopura, B L
Mishra, S P
Keywords: Melt-blending;Poly(butylene terephthalate);Poly(ethylene terephthalate);Polymer blending;Spinning
Issue Date: Mar-1988
Publisher: NISCAIR-CSIR, India
Abstract: The blend fibres prepared from poly( ethylene terephthalate) and 0-10% poly(butylene terephthalate) by sequential melt-blending and spinning show a single glass transition temperature, less than that of 100% PET. The melting point of the blend fibres is lower than that of 100% PET owing to decrease in crystalline order and partial transesterification. The thermal stability of the blend fibre decreases on addition of more than 3% PBT. Addition of 3% poly (butylene terephthalate) to poly(ethylene terephthalate) increases birefringence, initial modulus, sonic modulus and tenacity, which may be associated with higher inter-crystalline links.
Page(s): 23-25
ISSN: 0975-1025 (Online); 0971-0426 (Print)
Appears in Collections:IJFTR Vol.13(1) [March 1988]

Files in This Item:
File Description SizeFormat 
IJFTR 13(1) 23-25.pdf597.65 kBAdobe PDFView/Open


Items in NOPR are protected by copyright, with all rights reserved, unless otherwise indicated.