dc.description.abstractThe blend fibres prepared from poly (ethylene terephthalate) and 0-10% poly (butylene terephthalate) by simultaneous melt-blending and spinning show no transesterification. The crystalline orientation function of the blend fibres is same as that of 100% PET fibre. The amorphous orientation function is more influenced by phase stability and is minimum at the boundary of phase segregation. The crystalline, tenacity and modulus of the blend fibres improve owing to the formation of either tie chains, as in the case of 98/2 PET/PBT blend, or tie molecules, as in-the case of 90/10 PET/ PBT blend.en_US
dc.language.isoen_USen_US
dc.publisherNISCAIR-CSIR, Indiaen_US
dc.rights CC Attribution-Noncommercial-No Derivative Works 2.5 Indiaen_US
dc.sourceIJFTR Vol.13(4) [December 1988]en_US
dc.subjectMelt-blendingen_US
dc.subjectPoly(butylene terephthalate)en_US
dc.subjectPoly(ethylene terephthalate)en_US
dc.subjectPolymer blendingen_US
dc.subjectSpinningen_US
dc.titleModification of Poly(ethylene terephthalate) Fibre by Polymer Blending with Poly(butylene terephthalate) Fibre: Part III-Simultaneous Melt-blending and Spinningen_US
dc.typeArticleen_US
Appears in Collections:IJFTR Vol.13(4) [December 1988]

Files in This Item:
File Description SizeFormat 
IJFTR 13(4) 175-178.pdf952.89 kBAdobe PDFView/Open


Items in NOPR are protected by copyright, with all rights reserved, unless otherwise indicated.