Please use this identifier to cite or link to this item: http://nopr.niscpr.res.in/handle/123456789/32768
Full metadata record
DC FieldValueLanguage
dc.contributor.authorSom, N C-
dc.contributor.authorBagchi, A-
dc.contributor.authorMukherjee, A K-
dc.date.accessioned2015-10-19T06:55:14Z-
dc.date.available2015-10-19T06:55:14Z-
dc.date.issued1987-09-
dc.identifier.issn0975-1025 (Online); 0971-0426 (Print)-
dc.identifier.urihttp://hdl.handle.net/123456789/32768-
dc.description126-132en_US
dc.description.abstractJute fabrics undergo crosslinking reactions with N-methylol urea systems in the presence of catalysts and the modified fabrics show good wrinkle resistance along with other properties at the expense of tensile strength. The changes in properties of jute fabrics modified by crosslinking with DMEU and DMDHEU in the presence of acid catalysts are discussed.en_US
dc.language.isoen_USen_US
dc.publisherNISCAIR-CSIR, Indiaen_US
dc.rights CC Attribution-Noncommercial-No Derivative Works 2.5 Indiaen_US
dc.sourceIJFTR Vol.12(3) [September 1987]en_US
dc.subjectJute-based fabricsen_US
dc.subjectDimethylol dihydroxyethylene ureaen_US
dc.subjectDimethylol ethylene ureaen_US
dc.subjectN-Methylol ureaen_US
dc.subjectTensile strengthen_US
dc.subjectWrinkle recoveryen_US
dc.titleWrinkle Recovery and Tensile Strength of Jute-based Fabrics Modified by Treatment with N-Methylol System: Part II - Effect of Treatment in Presence of Acid Catalystsen_US
dc.typeArticleen_US
Appears in Collections:IJFTR Vol.12(3) [September 1987]