dc.description91-94en_US
dc.description.abstractTexturing of polyester-viscose blended yarn has been accomplished through heat setting of polyester and crosslinking of viscose by a single-stage rapid cure technique. Two resins, Finish KVS new (Sandoz) (dimethylol dihydroxycthy1cne urea based resin with built-in catalyst) and resin U-4750(BASF) (a polyfunctional urethane resin) were used as crosslinking agents for setting the deformation. The efficiency of both the resins has been studied as a function of curing period, temperature and catalyst and resin concentrations. It is observed that a curing temperature of 210-220oC and a curing period of 30 see are optimum for both the resins. With lesser amount of resin + catalyst in the padding bath, KVS gives a stronger yarn than U-4750 resin for an equivalent crimp rigidity value.en_US
dc.language.isoen_USen_US
dc.publisherNISCAIR-CSIR, Indiaen_US
dc.rights CC Attribution-Noncommercial-No Derivative Works 2.5 Indiaen_US
dc.sourceIJFTR Vol.04(3) [September 1979]en_US
dc.titleStudies on Texturing of Polyester Viscose Spun Yarn by Simultaneous Setting of Both the Componentsen_US
dc.typeArticleen_US
Appears in Collections:IJFTR Vol.04(3) [September 1979]

Files in This Item:
File Description SizeFormat 
IJFTR 4(3) 91-94.pdf994.82 kBAdobe PDFView/Open


Items in NOPR are protected by copyright, with all rights reserved, unless otherwise indicated.