Please use this identifier to cite or link to this item:
http://nopr.niscpr.res.in/handle/123456789/40208| Title: | Hydrothermal sealed tube reaction in the system, Na2O-SrO-SiO2-H2O : Formation of Na8Sr5Si16O41 |
| Authors: | Chakrabarty, K L |
| Issue Date: | Aug-1998 |
| Publisher: | NISCAIR-CSIR, India |
| Abstract: | A crystalline compound, 4Na2O-5SrO-16SiO2, has been synthesised by hydrothermal sealed tube reaction using strontium hydroxide hexahydrate. silica, sodium hydroxide and water as-starting materials at -120o C under a pressure of 14lb/ in2 for 28 h. The compound has been characterized by X-ray diffraction, IR, thermal studies and elemental analysis. Density and magnetic studies have also been carried out. |
| Page(s): | 715-717 |
| ISSN: | 0975-0975(Online); 0376-4710(Print) |
| Appears in Collections: | IJC-A Vol.37A(08) [August 1998] |
Files in This Item:
| File | Description | Size | Format | |
|---|---|---|---|---|
| IJCA 37A(8) 715-717.pdf | 220.23 kB | Adobe PDF | View/Open |
Items in NOPR are protected by copyright, with all rights reserved, unless otherwise indicated.